Modern solar modules are known for their brittle wafer-thin cells.
These cells can be as thin as 170 micrometres which is between 2 to 3 times the thickness of standard A4 paper.
To maximise the power potential of your solar system we have developed a short recommended handling guide to help get the most out of your solar system.
There are a few bad habits that can lead to performance drops during the installation process.
Below are a few examples of processes that can cause performance drops and the module handling techniques WINAICO recommends.
While many current installations require less than a full pallet of modules, we strongly recommend taking care when transporting materials on top of exposed modules.
A common example is an inverter strapped onto the top of multiple panels.
We tried to simulate the conditions of a drive with an inverter and a forklift.
Please avoid applying any force to the top of an open-air module during transport.
Strapping on the top of a pallet is suitable however pressure on the glass front or back sheet will cause irreparable damage during transportation.
Getting solar modules onto the roof will be one of the most strenuous tasks of installation.
As modules are moving to higher power classes, we are seeing an increased size and weight of modules making the issue more prevalent.
When moving modules onto a roof, we suggest using a mechanical lift but recognise that it is not always possible nor convenient.
Many of our partners move modules with ladders and we recommend trying to distribute the force against the modules.
The optimal scenarios for module handling with ladders are to allow the module to rest against the arm, shoulder, back and head as much as possible to distribute the load away from a localised place.
Incorrect module carrying shown above can reduce the power output instantaneously by almost 1%.
It is also common knowledge that standing on a module is a habit that must be avoided.
We have used before and after EL images to demonstrate the impact of one person standing on different points of the panel.
Two cells in the bottom right demonstrate distinct darkening.
The colour change suggests the development of microcracks and a loss of total module performance.
The power loss is around 7 watts or 2.2% of the power on a fully functional module.
This would propagate further under the influence of humidity, thermal expansion and contraction and usual wear and tear.
Please avoid any unnecessary force on the surface of the modules.
Cookie | Duration | Description |
---|---|---|
cookielawinfo-checkbox-analytics | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Analytics". |
cookielawinfo-checkbox-functional | 11 months | The cookie is set by GDPR cookie consent to record the user consent for the cookies in the category "Functional". |
cookielawinfo-checkbox-necessary | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookies is used to store the user consent for the cookies in the category "Necessary". |
cookielawinfo-checkbox-others | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Other. |
cookielawinfo-checkbox-performance | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Performance". |
viewed_cookie_policy | 11 months | The cookie is set by the GDPR Cookie Consent plugin and is used to store whether or not user has consented to the use of cookies. It does not store any personal data. |